MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American Black Cottonwood Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Hardwood. Relatively easy to work with hand tools. Fair steam bending, poor planing, poor shaping. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Populus trichocarpa; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.350 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 1100 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1200 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 270 psiPerpendicular to Grain*
Modulus of Rupture 0.0570 GPaIn Bending
 4.80 ksiStatic Bending*
Flexural Yield Strength 36.5 MPaBending stress at proportional limit
 2900 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 9.00 - 9.45 GPaIn Bending
 1070 ksiStatic Bending*
Compressive Strength 3.30 MPaPerpendicular to Grain
 30.3 - 34.0 MPaParallel to Grain
 200 psiPerpendicular to Grain*
 1770 psiParallel to Grain*
 2160 psiMax Crushing Strength Parallel to Grain*
Shear Strength 600 psiParallel to Grain*
Impact 2.2in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 6800psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.440 in-lb/in³Static Bending*
Work to Maximum Load 5.00 in-lb/in³Static Bending*
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.600 BTU-in/hr-ft²-°FOven Dry
 0.720 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 3.6 %Radial, from green to oven dry
 8.6 %Tangential, from green to oven dry
 12.4 %Volumetric, from green to oven dry

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Eastern Hemlock Wood
Mountain Hemlock Wood
Silver Maple (Water Maple, White Maple), Soft Wood
American Yellow Poplar Wood
Balsam Poplar Cottonwood Wood

PTSAQ / 71300

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.