MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Rynite® FR543 NC010 PET-GF43FR(17)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 40% Glass Reinforced

Material Notes: 43% Glass Reinforced, Flame Retardant, Polyethylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.79 g/ccISO 1183
Melt Density 1.61 g/cc
@Temperature 280 °C
Water Absorption 0.60 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.100 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4, 2577
 0.00050 cm/cm
@Treatment Temp. 80.0 °C,
Time 173000 sec
Postmolding shrinkage; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4, 2577
 0.0035 cm/cm
@Treatment Temp. 80.0 °C,
Time 173000 sec
Postmolding shrinkage; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 102ISO 2039-2
Hardness, Rockwell R 122ISO 2039-2
Tensile Strength at Break 170 MPaISO 527-1/-2
Elongation at Break 1.8 %ISO 527-1/-2
Tensile Modulus 17000 MPaISO 527-1/-2
Flexural Modulus 14500 MPaISO 178
Compressive Strength 230 MPaISO 604
Poissons Ratio 0.33
Shear Strength 60.0 MPaASTM D 732
Charpy Impact Unnotched 30.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 43.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Coefficient of Friction, Static 0.16against steel; ASTM 1894
 0.18against itself; ASTM 1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+15 ohmIEC 62631-3-2
Dielectric Constant 4.1
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.6
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 37.0 kV/mmIEC 60243-1
Dissipation Factor 0.0131
@Frequency 1e+6 Hz
IEC 62631-2-1
 0.0368
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 225 VIEC 60112
 250 - 399 VPLC 2; UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°CISO 11359-1/-2
 11.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ASTM E 831
CTE, linear, Transverse to Flow 80.0 µm/m-°CISO 11359-1/-2
 79.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ASTM E 831
Specific Heat Capacity 1.56 J/g-°C
@Temperature 280 °C
Melt
Thermal Conductivity 0.310 W/m-KSolid
 0.300 W/m-K
@Temperature 280 °C
Melt
Melting Point 254 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 240 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 225 °CISO 75-1/-2
Vicat Softening Point 225 °C50°C/h, 50N; ISO 306
Glass Transition Temp, Tg 90.0 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 V-0
@Thickness 0.800 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 5VA
@Thickness 1.50 mm
IEC 60695-11-20
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index 35 %ISO 4589-1/-2
Glow Wire Test 960 °C
@Thickness 0.750 mm
No Flame; IEC 60335-1
 960 °C
@Thickness 1.00 mm
No Flame; IEC 60335-1
 960 °C
@Thickness 1.50 mm
No Flame; IEC 60335-1
 960 °C
@Thickness 2.00 mm
No Flame; IEC 60335-1
 960 °C
@Thickness 3.00 mm
No Flame; IEC 60335-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °COptimum, Injection
 270 - 290 °CRange, Injection
Mold Temperature 110 °COptimum, Injection
 100 - 120 °CInjection
Ejection Temperature 170 °CInjection
Drying Temperature 120 °CInjection
Dry Time 4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %Injection
Hold Pressure >= 80.0 MPaInjection
 
Descriptive Properties
AdditivesFlame retardant
 Release agent
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PET-GF43FR(17)<ISO 11469
PolymerPET-GF43 FR(17)
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPET-GF43FR(17)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX4847 / 256296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.