MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Brewer Science BrewerBOND® 510 Temporary Bonding Material
Categories: Other Engineering Material

Material Notes: Temporary wafer bonding release material for mechanical debonding applications.

BrewerBOND® 510 material is applied to a carrier using a simple process and is compatible with =300°C bonding materials. After processing, a low-force separation method is used to debond, and the carrier could potentially be reused. Because the carrier may be reused (depending on metallization processes), this material has a lower cost of ownership than other options, making it ideal for entry into the wafer-bonding space or for projects with smaller throughput requirements.

Key Market Sectors include 3-D wafer-level packaging, MEMS, and Compound semiconductor.

Benefits include Compatible with 250°C - 300°C bonding materials; Simple application on carrier; Lower cost of ownership with carrier reuse; Carrier rework by RCA clean or ash; and Low-force separation.

Information provided by Brewer Science.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.00500 micronsSpin Speed 1700 rpm
 0.00620 micronsSpin Speed 1100 rpm
 0.00750 micronsSpin Speed 800 rpm
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 280 °C2% wt loss in TGA
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.23
@Wavelength 633 nm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 205 °C
@Time 60.0 sec
Proximity Bake
 
Descriptive Properties
Contact Angle with Water102 to 106°Room Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Brewer Science WaferBOND HT-10.10 Temporary Bonding Material
Brewer Science WaferBOND CR-220 Temporary Bonding Material
Brewer Science ProTEK® PSB Photosensitive Protective Coating
Brewer Science ProTEK® B3 Alkaline-Resistant Coating
Brewer Science BrewerBOND® 701 Laser Release Material

PBREW992 / 193508

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.