MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 52% Cold Worked
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts improved cleanliness. The chemistry modifications are designed to maximize the corrosion resistance of this alloy and provide a ferrite free microstructure. The alloy is nonmagnetic even after severe cold forming operations.

BioDur™ is a trademark of Carpenter Technology Corporation.

Key Words: ASTM F138 Grade 2; ASTM F139 Grade 2; ISO 5832-1 Composition D; Type 316 Stainless Steel
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.95 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 334Estimated from Rockwell C for Brinell test with 3000 kg load, 10 mm ball.
Hardness, Knoop 363Estimated from Rockwell C
Hardness, Rockwell C 36
Hardness, Vickers 349Estimated from Rockwell C
Tensile Strength, Ultimate 1034 MPa
Tensile Strength, Yield 848 MPa
@Strain 0.2 %
Elongation at Break 16 %
Reduction of Area 62 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000740 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.5 µm/m-°C
@Temperature 0.000 - 649 °C
Specific Heat Capacity 0.500 J/g-°C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 17 - 19 %
Copper, Cu <= 0.50 %
Iron, Fe 62 %as remainder
Manganese, Mn <= 2.0 %
Molybdenum, Mo 2.25 - 3.5 %
Nickel, Ni 13 - 15 %
Nitrogen, N <= 0.10 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.75 %
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 90% Cold Worked
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 35% Cold Worked
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 48% Cold Worked
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, Annealed
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 70% Cold Worked

NCAR53 / 15631

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.