MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Skamol Group SUPER 1100 E Calcium Silicate Insulating Slab
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: SKAMOL SUPER calcium silicate slabs have the following characteristics:
  • Max. service temperature: Up to 1100°C (2012°F)
  • Back-up insulation only
  • Extremely lightweight
  • Very low thermal conductivity
  • Excellent mechanical strength
  • Can be used in furnaces with reducing atmosphere due to their high resistance to carbon monoxide and hydrocarbons
  • Designed for the application as back-up insulation of all refractory constructions
  • The ideal choice for efficient insulation of kilns, furnaces, ovens, stoves, boilers, soaking pits, regenerators, mains and other combustion equipment
  • The combination of low weight, high service temperature and good integrity makes the calcium silicate slabs highly applicable as fire protection in several applications.

Information provided by Skamol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.245 g/cc0.00885 lb/in³Dry
Loss On Ignition 6.0 %
@Temperature 1025 °C
6.0 %
@Temperature 1877 °F
Porosity 90 %90 %Total
Permeability 0.500.50nPm, Permeability to Air; BS EN 993-4: 1995
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00180 GPa0.261 ksiEN 993-6: 1995
Compressive Strength 2.70 MPa392 psiEN 1094-5: 1995
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.50 µm/m-°C
@Temperature 20.0 - 750 °C
3.06 µin/in-°F
@Temperature 68.0 - 1380 °F
BS 1902: section 5.3: 1990
Specific Heat Capacity 0.840 J/g-°C0.201 BTU/lb-°F
Thermal Conductivity  0.0700 W/m-K
@Temperature 200 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 392 °F
Mean temp.; ASTM C-182
 0.0900 W/m-K
@Temperature 400 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C-182
 0.100 W/m-K
@Temperature 600 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C-182
Maximum Service Temperature, Air 1100 °C2010 °F
Shrinkage 1.5 %
@Time 43200 sec
1.5 %
@Time 12.0 hour
Linear Reheat Shrinkage, 12h at 50°C (122°F) below max. service temp.; EN 1094-6: 1999
 
Component Elements PropertiesMetricEnglishComments
Al2O3 0.30 %0.30 %
CaO 45 %45 %
Fe2O3 0.30 %0.30 %
K2O 0.10 %0.10 %
MgO 0.60 %0.60 %
Na2O 0.10 %0.10 %
SiO2 47 %47 %
 
Descriptive Properties
ColorGrey
Creep in Compression0.4 %BS EN 993-9: 1997, 50h at 900°C (1652°F), load 0.1 MPa (14.5 psi)
Pyrometric Cone Equivalent1345°CASTM C24-89, ORTON cones

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab
Sharadaa Ceramics Calcium Silicate Block
Hexcel® HexTow® AS4 3K Standard Modulus Carbon Fiber (3000 Filaments)
Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab
S-Glass Fiber, Generic

CSKAM013 / 2164

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.