MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Von Roll Isola IMI E-Solder® 3012 Electrically Conductive Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Data provided by Von Roll Isola USA.

E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue to contaminate sensitive electronic components.

Key Words: Von Roll Isola USA; Insulating Materials Incorporated
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 35.0 MPabutt tensile strength per ASTM D426 on brass
Adhesive Bond Strength 14.0 MPaTensile shear per ASTM D1002 on etched Al panel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000500 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 2.10 W/m-K
Maximum Service Temperature, Air 175 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 135 °CSuggested baking time at this temperature is 6-18 hr. May also be cured for shorter time at higher temperatures.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Von Roll Isola IMI E-Solder® 3017 Electrically Conductive Adhesive
Von Roll Isola IMI E-Solder® 3025 Electrically Conductive Adhesive
Von Roll Isola IMI E-Solder® 3021 Electrically Conductive Adhesive
Von Roll Isola IMI E-Solder® 3022 Electrically Conductive Adhesive
Von Roll Isola IMI E-Solder® 3026 Electrically Conductive Adhesive

PISO39 / 48442

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.