MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borcoat™ EA165E Elastomer Modified Polypropylene for Extrusion
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Borcoat EA165E is an elastomer modified compound, based on a high molecular weight copolymer. The elastomer modification gives excellent low temperature impact resistance.

Borcoat EA165E is recommended for sheet, pipe extrusion, pipe coating and thermoforming of industrial parts, either as such or as a coextruded layer. It is suitable for applications requiring excellent low temperature performance.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5959ISO 868
Tensile Strength, Yield 18.0 MPa2610 psiAt 50 mm/min; ISO 527-2
Elongation at Yield 4.0 %4.0 %At 50 mm/min; ISO 527-2
Flexural Modulus 0.800 GPa116 ksiAt 2 mm/min; ISO 178
Charpy Impact, Notched  6.50 J/cm²
@Temperature -20.0 °C
30.9 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 7.50 J/cm²
@Temperature 0.000 °C
35.7 ft-lb/in²
@Temperature 32.0 °F
ISO 179/1eA
 
Processing PropertiesMetricEnglishComments
Front Barrel Temperature 210 - 230 °C410 - 446 °F
Die Temperature 230 - 240 °C446 - 464 °F
Melt Temperature 230 - 240 °C446 - 464 °F
Head Temperature 230 - 240 °C446 - 464 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BA11CF Polypropylene Copolymer
Overview of materials for Polypropylene, Film Grade
Borealis HL504FB Polypropylene Homopolymer
Borealis BH374MO Polypropylene Copolymer
Borealis Borstar® CB9600 HDPE for Extrusion Coating

PBOREA046 / 27353

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.