System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Pocan® T 7391 POS151 900044 PBT+PET, 45% Glass Fiber Filled
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
PBT + PET Blend, Glass Filled
Material Notes:
PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Bulk Density
0.800
g/cc
ISO 60
Density
1.69
g/cc
ISO 1183
Moisture Absorption at Equilibrium
0.10 %
50% RH; ISO 62
Water Absorption at Saturation
0.30 %
ISO 62
Viscosity Test
80
cm³/g
Viscosity Number; ISO 1628-5
Linear Mold Shrinkage, Flow
0.0020
cm/cm
60x60x2; 270 °C / MT 90°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0080
cm/cm
60x60x2; 270 °C / MT 90°C; 600 bar; ISO 294-4
Melt Flow
30
g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133-1
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
250
MPa
ISO 2093-1
Tensile Strength at Break
160
MPa
5 mm/min; ISO 527-1,-2
Elongation at Break
1.9 %
5 mm/min; ISO 527-1,-2
Tensile Modulus
16000
MPa
1 mm/min; ISO 527-1,-2
Flexural Strength
260
MPa
2 mm/min; ISO 178-A
Flexural Modulus
15500
MPa
2 mm/min; ISO 178-A
Flexural Strain at Break
2.1 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO)
55.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1U
60.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched
60.0
kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
65.0
kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
Charpy Impact, Notched
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
Tensile Creep Modulus, 1 hour
16500
MPa
ISO 899-1
Tensile Creep Modulus, 1000 hours
15000
MPa
ISO 899-1
Electrical Properties
Original Value
Comments
Dielectric Constant
4.2
@Frequency 1e+6 Hz
IEC 60250
4.3
@Frequency 100 Hz
IEC 60250
Dielectric Strength
28.0
kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor
0.0020
@Frequency 100 Hz
IEC 60250
0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
250
V
Solution A; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
20.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow
80.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Thermal Conductivity
0.270
W/m-K
ISO 8302
Melting Point
225
-
250
°C
10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air
150
°C
20000 h (Tensile impact strength); IEC 60216-1
155
°C
20000 h (Tensile strength); IEC 60216-1
155
°C
20000 h (Electric strength); IEC 60216-1
Hot Ball Pressure Test
220
°C
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
225
°C
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
206
°C
ISO 75-1,-2
Deflection Temperature at 8.0 MPa
150
°C
ISO 75-1,-2
Vicat Softening Point
210
°C
@Load 5.10 kg
120°C/h; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.800 mm
Oxygen Index
21 %
Method A; ISO 4589-2
Glow Wire Flammability Index
750
°C
@Thickness 2.00 mm
IEC 60695-2-12
Shrinkage, MD
0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
Flow Direction Post-Molding, 60x60x2; ISO 294-4
Shrinkage, TD
0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Molding, 60x60x2; ISO 294-4
Processing Properties
Original Value
Comments
Melt Temperature
270
°C
injection molding; ISO 294
260
-
280
°C
Mold Temperature
90.0
°C
injection molding; ISO 294
80.0
-
100
°C
Drying Temperature
120
°C
Dry Time
4.00
-
8.00
hour
Moisture Content
0.00 - 0.020 %
Karl Fischer
Descriptive Properties
Specifications
10.2°C
Halving interval (Electric strength), IEC 60216-1
10.2°C
Halving interval (Tensile strength), IEC 60216-1
13.5°C
Halving interval (Tensile impact strength), IEC 60216-1
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Asahi Kasei Leona™ 91G60 Polyamide 66, MF Reinforced
Envalior Durethan® BKV 240 H2.0 XCP 901510 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 50 H2.0 901510 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Dry
Celanese Crastin® SK605 NC010 PBT-GF30
Celanese Crastin® SK603 BK851 PBT-GF20
PLANW9198 / 208473
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.