MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Honeywell Stretch-Vac® Elastomax 1000 Heat-Stabilized Blown Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: Capran® Elastomax 1000 is a pink tinted, heat-stabilized blown film produced from modified nylon resin. It is available in widths up to 80 inches as layflat tubing and 120 inches as slit tubing. Thickness is 2.00 mils. In addition, it has excellent heat stability and resistance to pinholing. It can be used at temperatures up to 400°F (204°C) for typical composite cure cycle times.

Applications: Capran® Elastomax 1000 blown film is recommended as bagging film for advanced composite fabrication and other high temperature applications where softness, workability or anti-static characteristics are essential.

Information provided by Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0860 lb/in³Yield Density
Thickness 1.00 mil
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 4700 psiASTM D882
Film Tensile Strength at Yield, TD 4100 psiASTM D882
Film Elongation at Break, MD 400 %ASTM D882
Film Elongation at Break, TD 400 %ASTM D882
Secant Modulus, MD 0.469 GPaASTM D882
Secant Modulus, TD 0.476 GPaASTM D882
Tear Strength Test 530graves tear MD, grams/mil; ASTM D1004
 600graves tear TD, grams/mil; ASTM D1004
Elmendorf Tear Strength, MD 95.0 g/mil
Elmendorf Tear Strength, TD 95.0 g/milASTM D1922
Film Tensile Strength at Break, MD 14500 psiASTM D882
Film Tensile Strength at Break, TD 11000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 211 °Ccrystalline melting point; DSC
Shrinkage, MD <= 1.0 %
@Treatment Temp. 177 °C,
Time 601 sec
ASTM D1204
Shrinkage, TD <= 1.0 %
@Treatment Temp. 177 °C,
Time 601 sec
ASTM D1204

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALS00 / 23999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.