MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Titanium Ti-6Al-2Sn-4Zr-2Mo-0.1Si; Duplex Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: Information provided by Allvac and the references.

Excellent creep resistance, good tensile strength, toughness and high temperature stability. Properties highly dependent on heat treatment.

Applications: High-temp jet engines. Blades, discs, spacers, seals. High performance automotive valves.

Forms Typically available: Billet, bar, plate, sheet, strip and extrusions.

Key Words: Ti-6242Si; Ti-6242S; UNS R54620
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.54 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 318Estimated from Rockwell C.
Hardness, Knoop 346Estimated from Rockwell C.
Hardness, Rockwell C 34
Hardness, Vickers 333Estimated from Rockwell C.
Tensile Strength, Ultimate 1110 MPa
Tensile Strength, Yield 1050 MPa
Elongation at Break 13 %
Reduction of Area 30 %
Modulus of Elasticity 118 GPa
Compressive Modulus 118 GPa
Notched Tensile Strength 1025 MPaKt >17; Average of longitudinal and transverse.
Ultimate Bearing Strength 1800 MPae/D = 2.0; varies with thickness; this value is at about 2.4 mm.
Bearing Yield Strength 1450 MPae/D = 2.0
Poissons Ratio 0.325
Fatigue Strength 225 MPa
@# of Cycles 1.00e+7
Kt = 3
 320 MPa
@# of Cycles 50000
Kt = 3
 610 MPa
@# of Cycles 1.00e+7
A=0.67
 750 MPa
@# of Cycles 500000
A = 0.67
Shear Modulus 44.5 GPaCalculated
Charpy Impact 36.0 JV-Notch, oxygen content about 0.1%. Value drops with increasing O content.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000190 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.70 µm/m-°C
@Temperature 0.000 - 100 °C
 7.70 µm/m-°C
@Temperature 205 °C
 8.10 µm/m-°C
@Temperature 315 - 540 °C
average
Specific Heat Capacity 0.460 J/g-°C
Thermal Conductivity 7.00 W/m-K
Melting Point <= 1705 °C
Liquidus 1705 °C
Maximum Service Temperature, Air 425 °Ccontinuous use
 565 °Cintermittent use
Beta Transus 995 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.5 - 6.5 %
Carbon, C <= 0.050 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.25 %
Molybdenum, Mo 1.8 - 2.2 %
Nitrogen, N <= 0.050 %
Other, each <= 0.10 %
Other, total <= 0.30 %
Oxygen, O <= 0.15 %
Silicon, Si 0.060 - 0.10 %
Tin, Sn 1.8 - 2.2 %
Titanium, Ti 83.785 - 87.24 %As Balance; Elemental Composition per ASTM B265
Zirconium, Zr 3.6 - 4.4 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® 6-2-4-2 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age
Titanium Ti-6Al-2Sn-4Zr-2Mo (Ti-6-2-4-2), Duplex Annealed
Titanium, Ti
Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si)
Titanium Ti-8Al-1Mo-1V (Ti-8-1-1), Beta Solution Treated

MTA081 / 14114

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.