MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sumitomo Bakelite Varcum 92600 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Varcum 92600 is a liquid one-step phenolic resin in ethanol

APPLICATION: Varcum 92600 is an unmodified phenolic resin solution producing baked films that are outstanding in resistance to almost all acids, salt and fresh water, solvents, oils and other organic chemicals. They have good durability and abrasion resistance. Varcum 92600 is a fast curing resin solution, and the relatively low temperature and short time necessary for its polymerization result in light colored films. Baked films of Varcum 92600 can be plasticized sufficiently to enable them to withstand shocks or rough handling.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 4.54.5DCT 4064A
Viscosity 805 cP
@Temperature 25.0 °C
805 cP
@Temperature 77.0 °F
DCT 4003F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 3.5<= 3.5G-H; DCT 4075A
 
Descriptive Properties
Non Volatile (%)55DCT 4005A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Varcum 29353 Phenolic Resin
Sumitomo Bakelite Varcum 29109 Phenolic Resin

PSUMIT734 / 194539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.