MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions 81530 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, 30% Glass Fiber Reinforced

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.62 g/cc1.62 g/ccASTM D792
Spiral Flow 63.5 cm25.0 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888ASTM D2240
Tensile Strength, Yield 103 MPa14900 psiType I, 51 mm/min; ASTM D638
Elongation at Break 2.0 %2.0 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 9.65 GPa1400 ksiType I, 51 mm/min; ASTM D638
Flexural Strength 159 MPa23100 psiASTM D790
Flexural Modulus 9.31 GPa1350 ksiASTM D790
Poissons Ratio 0.400.40ASTM E132
Shear Modulus 3.45 GPa500 ksiCalculated
Izod Impact, Notched 1.10 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
2.06 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Izod Impact, Unnotched 2.70 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
5.06 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D4812
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 77.8 °C
@Thickness 6.35 mm
172 °F
@Thickness 0.250 in
Annealed; ASTM D648
UL RTI, Electrical 50.0 °C122 °FUL 746
UL RTI, Mechanical with Impact 50.0 °C122 °FUL 746
UL RTI, Mechanical without Impact 50.0 °C122 °FUL 746
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
ALL; UL 94
 5VA
@Thickness 1.50 mm
5VA
@Thickness 0.0591 in
ALL; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 - 210 °C390 - 410 °F
 
Descriptive Properties
Agency RatingsNSF 61
FeaturesGeneral Purpose
 High Flow
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
ReinforcementGlass Fiber, 30% by Weight
UsesFluid Handling
 General Purpose

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions 81510 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 80530 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 83510 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 81520 Polyvinyl Chloride, Rigid
Axiall LR-5009 Rigid PVC, Molding, All Colors

PH0POL0146 / 144715

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.