MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2)
Categories: Ceramic; Oxide; Aluminum Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Te value is 670°C. Hasselman Thermal Shock value is 800 K.

Data provided by CeramTec North America.

Key Words: 2MgO-2Al2O3-5SiO2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.30 g/cc
Water Absorption 5.0 - 7.0 %
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 640HV 0.5
Tensile Strength, Ultimate 25.5 MPaACMA Test #4
Modulus of Elasticity 128 GPaUltrasonic
Flexural Strength 82.6 MPa20 x 40 mm
Compressive Strength 275 MPaASTM C773-88
Poissons Ratio 0.28ASTM C-1 259-94
Shear Modulus 51.0 GPaUltrasonic
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 780000 ohm-cm
@Temperature 700 °C
 1.00e+14 ohm-cm
@Temperature 25.0 °C
Dielectric Constant 5.2
@Frequency 1e+6 Hz
Dielectric Strength 6.772 kV/mm
@Thickness 6.35 mm
Dissipation Factor 0.010
@Frequency 1e+6 Hz
Dielectric Loss Index 0.052
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.30 µm/m-°C
@Temperature 25.0 - 300 °C
 3.00 µm/m-°C
@Temperature 25.0 - 700 °C
 3.20 µm/m-°C
@Temperature 25.0 - 1001 °C
Specific Heat Capacity 0.700 J/g-°C
Thermal Conductivity 1.60 W/m-K
Maximum Service Temperature, Air 1100 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cordierite, 2MgO-2Al2O3-5SiO2
China-Yixing Longly Refractories ASM-120 Cordierite-Mullite
CeramTec 447 Cordierite
Morgan Advanced Ceramics Cordierite
China-Yixing Longly Refractories ASM-130 Cordierite-Mullite

CCERA4 / 671

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.