MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Corning ULE® 7973 EUV Standard Grade Ultra Low Expansion Glass
Categories: Ceramic; Glass; Optical

Material Notes: 7973 is a titania-silicate low expansion glass that has been tailored to meet the needs for mask and optical substrates for EUVL applications. 7973 has a similar composition to ULE® 7972 glass and is made using the same flame deposition process. The lithography transition from 193nm to 13.4nm required a major design shift in stepper optics from refractive to reflective. In reflective optics, substrate materials should be purely passive. The incident light should reflect off of the multilayer coatings of the optics and the photomask without the introduction of any mechanical or optical distortion caused by the underlying substrate. To minimize distortion from the minute temperature changes and meet the stringent EUVL specifications, the substrates must have a near-zero coefficient of thermal expansion (CTE) and tightly controlled zero cross over range.

Excellent resistance to weathering. Exhibits virtually no surface clouding or electrical surface leakage when subjected to attack by water, sulfur dioxide, and other atmospheric gases. High resistance to attack by nearly all chemical agents.

ULE® 7973 comes in several grades with varying size/levels of inclusions and striae; CTE control, and birefringence. The distinguishing attributes of the EUV Standard Grade are low birefringence; Tzc specified; low striae; and low inclusions in the critical zone; and CTE Zero Cross Over Temperature 20°C ± 10°C.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.21 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 460kg/mm² at 200g load
Tensile Strength, Ultimate 49.8 MPa
Modulus of Elasticity 67.6 GPa
Bulk Modulus 34.1 GPa
Poissons Ratio 0.17
Shear Modulus 29.0 GPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+11 ohm-cm
@Temperature 200 °C
100Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear -0.700 µm/m-°C
@Temperature -150 °C
Approximate Instantaneous Value
 -0.400 µm/m-°C
@Temperature -100 °C
Approximate Instantaneous Value
 -0.190 µm/m-°C
@Temperature -50.0 °C
Approximate Instantaneous Value
 -0.0300 µm/m-°C
@Temperature 3.00 °C
Approximate Instantaneous Value
 -0.0300 - 0.0300 µm/m-°C
@Temperature 5.00 - 35.0 °C
Specified mean from 5 to 35°C
 0.0300 µm/m-°C
@Temperature 42.5 °C
Approximate Instantaneous Value
 0.0500 µm/m-°C
@Temperature 250 °C
Approximate Instantaneous Value
 0.0800 µm/m-°C
@Temperature 200 °C
Approximate Instantaneous Value
 0.0800 µm/m-°C
@Temperature 100 °C
Approximate Instantaneous Value
 0.0900 µm/m-°C
@Temperature 150 °C
Approximate Instantaneous Value
Specific Heat Capacity 0.767 J/g-°C
Thermal Conductivity 1.31 W/m-K
Softening Point 1490 °C
Annealing Point 1000 °C
Strain Point 890 °C
 
Optical PropertiesOriginal ValueComments
Abbe Number 53.1vd
 
Descriptive Properties
Birefringence< 20 nm/cm
Stress Optical Coefficient4.15 (nm/cm)/(kg/cm²)
Striae100Non-Critical Zone. 0 to 400 Scale (%)
 50Critical Zone. 0 to 400 Scale (%)
Thermal Diffusivity.0079 cm²/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ceradyne Ceralloy® 147-1B Reaction Bonded Silicon Nitride (Si3N4)
Ceradyne Ceralloy® 147-A Hot Pressed Silicon Nitride (Si3N4)
Ceradyne Ekatherm EKasin® S Gas Pressure Sintered Silicon Nitride (Si3N4)
Corning Pyrex® 7740 Borosilicate Glass Sheet
Quartz (SiO2)

CCORNG974 / 233289

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.