- Available in North America
- Additive: Heat Stabilizer and Lubricant
- Features: Lubricated, Heat Stabilized, High Flow and Ultra High Toughness
- RoHS Compliant
- Auto Specifications: DELPHI DCM 4849 Color: Black, FORD WSK-M4D666-A Color: Black, FORD WSK-M4D666-A Color: Natural
- Form: Pellets
- Processing Method: Injection Molding