MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos H01H-00 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: This is a low flow rate homopolymer designed for extrusion or injection molding. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

    Applications
  • Injection molded articles
  • Extruded sheet and profiles

    Benefits
  • Stabilized for long term heat aging

Information provided by Ineos Olefins & Polymers USA

Key Words: Low flow rate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.909 g/ccASTM D792
Melt Flow 1.7 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 95ASTM D785
Tensile Strength at Break 2900 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 4900 psi2.0 in/min; ASTM D638
Elongation at Break 120 %2.0 in/min; ASTM D638
Elongation at Yield 13 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 200000 psiASTM D790A
Izod Impact, Notched 0.900 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 2.24 ft-lb/in²Area; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 199 °FUnannealed; ASTM D648
Vicat Softening Point 305 °FASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ProcessExtrusion
 Injection Molding
 Sheet Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos R35C-01 Polypropylene Random Copolymer
Ineos R35C-00 Polypropylene Random Copolymer
Ineos R01C-00 Polypropylene Random Copolymer
Ineos R12C-00 Polypropylene Random Copolymer
Ineos R12C-01 Polypropylene Random Copolymer

PINEOS016 / 99337

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.