MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CIMBAR BARA 325 Barium Sulfate (BaSO4)
Categories: Ceramic; Other Engineering Material; Additive/Filler for Polymer

Material Notes: BARA 200 is a natural, off-white barium sulfate. Cimbar's BARA 325 is a clean, high purity, high specific gravity, low solubility barium sulfate and it is chemically inert. These properties have made BARA 325 the industry standard for quality and performance in a wide range of other end-use applications.

Information provided by Cimbar Performance Minerals.

Key Words: BaSO4, Baryte, Barite
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 4.20 g/cc
Oil Absorption 9.0 - 10 %
Moisture Absorption at Equilibrium <= 0.10 %
Particle Size 10 µmMedian
Particle Mesh Size 200 Mesh99.8% passing
 325 Mesh98.5% passing
pH 8.0
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 1.4 %
SiO2 2.0 %
 
Descriptive Properties
BaSO4 (%)94
SrSO4 (%)0.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CIMBAR BARA 200 Barium Sulfate (BaSO4)
CIMBAR BariScan Elite Chemically Purified White Barium Sulfate (BaSO4)
CIMBAR CIMTUFF® 9102 Talc
CIMBAR Miti-Wite B1 Chemically Purified White Barite (BaSO4)
CIMBAR CIMTUFF® 9103 Talc

CIMBAR919 / 133401

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.