MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestodur® CL2012 12% Glass Reinforced, Crosslinkable PBT Based Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Description: VESTODUR CL2012 is a 12 % glass fiber reinforced, self-extinguishing compound for injection molding, based on modified polybutylene terephthalate (PBT). Moldings of VESTODUR CL2012 can be crosslinked by high-energy radiation or heat. The radiation will not influence the mechanical properties significantly. The short-term heat resistance is increased up to 320 °C depending on the conditions. Therefore, crosslinked parts of VESTODURCL2012 can be used, for example, in common soldering processes in the electronic industry as surge soldering, gas phase soldering or IR soldering.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccISO 1183
Water Absorption at Saturation 0.40 %ISO 62
Linear Mold Shrinkage 0.005 cm/cm
@Thickness 2.00 mm
sheet with film gate at rim, mold temperature 80°C
Linear Mold Shrinkage, Transverse 0.018 cm/cm
Melt Flow 41.08 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527-1/2
Elongation at Break 2.0 %ISO 527-1/2
Tensile Modulus 5.80 GPaISO 527-1/-2
Charpy Impact Unnotched 3.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
 3.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.650 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 0.650 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Strength 30.0 kV/mmK20/P50; IEC 60243-1
Comparative Tracking Index 175 V100 drops value; IEC 60112
 200 VTest Solution A CTI; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 213 °CMethod A, 10 N; ISO 75-1/-2
Flammability, UL94 V-0
@Thickness 0.800 mm
IEC 60695
 V-0
@Thickness 1.60 mm
IEC 60695

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 912BA Thermoplastic Elastomer
Mocom (ALBIS) ALCOM® PBT 700/1 GF20 PTFE15 PBT, 20% Glass/15% PTFE Reinforced
Celanese Crastin® CE15315 BK010 PBT-GF15FR(17)
Borealis BorPURE™ RE450MO Polypropylene Random Copolymer
Borealis BA11CF Polypropylene Copolymer

PHUMA13 / 47527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.