MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Reynolds EA-40® Clear Amber Epoxy Adhesive and Laminating Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: EA-40® Clear Amber Epoxy is an unfilled low-viscosity epoxy adhesive that can be spread easily in thin films that are almost transparent after curing. EA-40® has a long pot life and cures in 24 hours at room temperature to provide good mechanical and electrical properties. Mix ratio is 1:1 by volume. When mixed 2A:1B by volume, EA-40® will achieve greater heat resistance and improved physical properties. EA-40® is versatile and can be used for many different assembly and repair applications ranging from electrical potting to jewelry assembly to repairing plumbing fixtures. Bow makers have come to know EA-40® as a tremendous laminating resin. EA-40® provides highly moisture resistant bonds meeting the performance requirements for Federal Specification MMM-A-188, Type III.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 66935
Tensile Strength 3400 psi
Elongation at Break 1.0 %
Modulus of Elasticity 140 ksiCompression
 190 ksiTension
Compressive Yield Strength 8100 psi
Adhesive Bond Strength 1400 psi
@Temperature -50.0 °C
Exposure: None; Substrate: AL 2024-T-3; ASTM D1002
 1500 psi
@Temperature 25.0 °C
Exposure: None; Substrate: AL 2024-T-3; ASTM D1002
 1800 psi
@Temperature 80.0 °C
Exposure: None; Substrate: AL 2024-T-3; ASTM D1002
 2500 psi
@Temperature 25.0 °C
Exposure: 30 days in tap water @ 25°C; Substrate: AL 2024-T-3; ASTM D1002
 2900 psi
@Temperature 25.0 °C
Exposure: 7 days in 100% RH @ 65°C; Substrate: AL 2024-T-3; ASTM D1002
 3300 psi
@Temperature 25.0 °C
Exposure: None; Substrate: Cold Rolled Steel; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 73.0 °CDeflection Temp. At 1A:1B Mix Ratio
 103 °CDeflection Temp. At 2A:1B Mix Ratio
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
Pot Life 120 min
 
Descriptive Properties
ColorClear Amber
Mix Ratio1A:1Bby volume
Mixed ViscosityLight-paste
Sag Resistance1/16”

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN293 / 296994

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.