MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polikim ULPOLEN® 1000 UHMWPE, Oil
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: The solid lubricant additive reduces Ulpolen®'s coefficient of friction even further. As the additive is dry, it does not accumulate dust or dirt. In conveyor belts, it reduces squeakings at corners and turns. Especially in bottling, it helps reduce material waste and noise.

Information provided by Polikim Polimer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccISO 1183
Molecular Weight 9.20e+6 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64ISO 868
Tensile Strength, Ultimate 214 kg(f)/cm²ISO 527-1
Elongation at Break >= 50 %ISO 527-1
Tensile Modulus 850 MPaISO 527-1
Coefficient of Friction 0.070
Sand Slurry 90
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmDIN VDE 0303
Surface Resistance 1.00e+12 ohmDIN VDE 0303
Arc Resistance 180 - 240 secDIN VDE 0303
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 20.0 - 100 °C
DIN 53752
Melting Point 133 - 138 °C
Maximum Service Temperature, Air 80.0 °Ccontinuous
 130 °Cshort term
Minimum Service Temperature, Air -250 °C
 -250 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMODUR® 0363 + BAYTEC® XL 0328 + BAYTEC® 0354 + BAYTEC® 0340 73A Polyurethane, MDI PPG
BASF 1,4-Butanediol (BDO)
Boric Acid (orthoboric acid), B(OH)3
Celanese GUR® 2122 PE-UHMW, Specialty
Avient LubriOne™ NN-30GF/13T-2S Black Polyamide 66 (Nylon 66)

PPOLIK020 / 99830

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.