MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Impact Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.13 - 1.73 g/cc0.0408 - 0.0625 lb/in³Average value: 1.31 g/cc Grade Count:69
 1.03 - 1.17 g/cc
@Temperature 250 - 250 °C
0.0372 - 0.0423 lb/in³
@Temperature 482 - 482 °F
Average value: 1.10 g/cc Grade Count:2
Filler Content 10.0 - 30.0 %10.0 - 30.0 %Average value: 18.3 % Grade Count:4
Water Absorption 0.0500 - 0.350 %0.0500 - 0.350 %Average value: 0.116 % Grade Count:12
Moisture Absorption at Equilibrium 0.0500 - 0.400 %0.0500 - 0.400 %Average value: 0.178 % Grade Count:16
Water Absorption at Saturation 0.200 - 0.800 %0.200 - 0.800 %Average value: 0.420 % Grade Count:5
Maximum Moisture Content 0.0200 - 0.04000.0200 - 0.0400Average value: 0.0240 Grade Count:5
Linear Mold Shrinkage 0.00160 - 0.0300 cm/cm0.00160 - 0.0300 in/inAverage value: 0.0155 cm/cm Grade Count:48
 0.00400 - 0.00400 cm/cm
@Temperature 80.0 - 80.0 °C
0.00400 - 0.00400 in/in
@Temperature 176 - 176 °F
Average value: 0.00400 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.00160 - 0.0300 cm/cm0.00160 - 0.0300 in/inAverage value: 0.0156 cm/cm Grade Count:20
 0.00900 - 0.00900 cm/cm
@Temperature 80.0 - 80.0 °C
0.00900 - 0.00900 in/in
@Temperature 176 - 176 °F
Average value: 0.00900 cm/cm Grade Count:2
Melt Flow 2.00 - 73.8 g/10 min2.00 - 73.8 g/10 minAverage value: 18.4 g/10 min Grade Count:27
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 104 - 120104 - 120Average value: 113 Grade Count:12
Hardness, Shore D 65.0 - 70.065.0 - 70.0Average value: 66.7 Grade Count:3
Tensile Strength, Ultimate 27.6 - 145 MPa4000 - 21000 psiAverage value: 56.9 MPa Grade Count:40
Tensile Strength, Yield 27.0 - 135 MPa3920 - 19600 psiAverage value: 49.4 MPa Grade Count:40
Elongation at Break 1.50 - 180 %1.50 - 180 %Average value: 42.1 % Grade Count:52
Elongation at Yield 3.00 - 130 %3.00 - 130 %Average value: 14.6 % Grade Count:13
Modulus of Elasticity 1.45 - 17.0 GPa210 - 2470 ksiAverage value: 3.36 GPa Grade Count:32
Flexural Yield Strength 45.0 - 172 MPa6530 - 25000 psiAverage value: 79.1 MPa Grade Count:46
Flexural Modulus 1.45 - 7.58 GPa210 - 1100 ksiAverage value: 2.44 GPa Grade Count:51
Poissons Ratio 0.390 - 0.4200.390 - 0.420Average value: 0.410 Grade Count:3
Izod Impact, Notched 0.374 J/cm - NB0.700 ft-lb/in - NBAverage value: 3.62 J/cm Grade Count:39
 2.24 - 7.4746 J/cm
@Temperature -40.0 - -28.9 °C
4.20 - 14.003 ft-lb/in
@Temperature -40.0 - -20.0 °F
Average value: 4.31 J/cm Grade Count:3
Izod Impact, Unnotched 18.7 J/cm - NB35.0 ft-lb/in - NBAverage value: 18.7 J/cm Grade Count:7
Izod Impact, Notched (ISO) 4.00 - 75.6 kJ/m²1.90 - 36.0 ft-lb/in²Average value: 28.2 kJ/m² Grade Count:17
 6.00 - 20.0 kJ/m²
@Temperature -40.0 - -30.0 °C
2.86 - 9.52 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 10.5 kJ/m² Grade Count:12
Izod Impact, Unnotched (ISO) 65.0 kJ/m² - NB30.9 ft-lb/in² - NBAverage value: 65.0 kJ/m² Grade Count:8
 60.0 kJ/m² - NB
@Temperature -40.0 - -30.0 °C
28.6 ft-lb/in² - NB
@Temperature -40.0 - -22.0 °F
Average value: 193 kJ/m² Grade Count:8
Charpy Impact Unnotched 6.50 J/cm² - NB30.9 ft-lb/in² - NBAverage value: 6.50 J/cm² Grade Count:13
 6.50 J/cm² - NB
@Temperature -40.0 - -30.0 °C
30.9 ft-lb/in² - NB
@Temperature -40.0 - -22.0 °F
Average value: 21.0 J/cm² Grade Count:12
Charpy Impact, Notched 1.00 - 9.00 J/cm²4.76 - 42.8 ft-lb/in²Average value: 4.16 J/cm² Grade Count:17
 0.900 - 2.50 J/cm²
@Temperature -40.0 - -20.0 °C
4.28 - 11.9 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 1.27 J/cm² Grade Count:12
Gardner Impact 36.2 - 36.2 J26.7 - 26.7 ft-lbAverage value: 36.2 J Grade Count:8
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+11 - 1.00e+17 ohm-cm1.00e+11 - 1.00e+17 ohm-cmAverage value: 1.90e+16 ohm-cm Grade Count:24
Surface Resistance 1.00e+6 - 1.00e+15 ohm1.00e+6 - 1.00e+15 ohmAverage value: 3.21e+14 ohm Grade Count:15
Dielectric Constant 3.00 - 3.703.00 - 3.70Average value: 3.40 Grade Count:6
Dielectric Strength 15.7 - 36.0 kV/mm400 - 914 kV/inAverage value: 25.5 kV/mm Grade Count:16
Dissipation Factor 0.00109 - 0.02400.00109 - 0.0240Average value: 0.0137 Grade Count:4
Arc Resistance 110 - 130 sec110 - 130 secAverage value: 119 sec Grade Count:4
Comparative Tracking Index 225 - 600 V225 - 600 VAverage value: 525 V Grade Count:9
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.2 - 190 µm/m-°C14.0 - 106 µin/in-°FAverage value: 103 µm/m-°C Grade Count:15
 233 - 233 µm/m-°C
@Temperature 55.0 - 160 °C
129 - 129 µin/in-°F
@Temperature 131 - 320 °F
Average value: 233 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 100 - 190 µm/m-°C55.6 - 106 µin/in-°FAverage value: 135 µm/m-°C Grade Count:8
 191 - 191 µm/m-°C
@Temperature 55.0 - 160 °C
106 - 106 µin/in-°F
@Temperature 131 - 320 °F
Average value: 191 µm/m-°C Grade Count:1
Specific Heat Capacity 2.10 - 2.10 J/g-°C
@Temperature 250 - 250 °C
0.502 - 0.502 BTU/lb-°F
@Temperature 482 - 482 °F
Average value: 2.10 J/g-°C Grade Count:1
Thermal Conductivity 0.200 - 0.200 W/m-K
@Temperature 250 - 250 °C
1.39 - 1.39 BTU-in/hr-ft²-°F
@Temperature 482 - 482 °F
Average value: 0.200 W/m-K Grade Count:1
Melting Point 210 - 255 °C410 - 491 °FAverage value: 225 °C Grade Count:27
Maximum Service Temperature, Air 80.0 - 105 °C176 - 221 °FAverage value: 96.7 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 225 °C194 - 437 °FAverage value: 142 °C Grade Count:44
Deflection Temperature at 1.8 MPa (264 psi) 48.0 - 210 °C118 - 410 °FAverage value: 80.5 °C Grade Count:57
Vicat Softening Point 105 - 215 °C221 - 419 °FAverage value: 163 °C Grade Count:10
Glass Transition Temp, Tg 55.0 °C131 °FAverage value: 55.0 °C Grade Count:3
UL RTI, Electrical 75.0 - 130 °C167 - 266 °FAverage value: 112 °C Grade Count:3
UL RTI, Mechanical with Impact 75.0 - 130 °C167 - 266 °FAverage value: 112 °C Grade Count:3
UL RTI, Mechanical without Impact 75.0 - 110 °C167 - 230 °FAverage value: 87.2 °C Grade Count:3
Flammability, UL94 HB - V-0HB - V-0Grade Count:48
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 778 °C Grade Count:6
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 280 °C446 - 536 °FAverage value: 254 °C Grade Count:13
Nozzle Temperature 225 - 280 °C437 - 536 °FAverage value: 249 °C Grade Count:11
Melt Temperature 190 - 280 °C374 - 536 °FAverage value: 249 °C Grade Count:33
Mold Temperature 10.0 - 130 °C50.0 - 266 °FAverage value: 72.7 °C Grade Count:39
Drying Temperature 80.0 - 140 °C176 - 284 °FAverage value: 118 °C Grade Count:37
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.0674 % Grade Count:17
Dew Point -40.0 - -28.9 °C-40.0 - -20.0 °FAverage value: -32.6 °C Grade Count:3
Injection Pressure 44.1 - 103 MPa6400 - 15000 psiAverage value: 74.8 MPa Grade Count:6
Vent Depth 0.00127 - 0.00381 cm0.000500 - 0.00150 inAverage value: 0.00145 cm Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant

O3202 / 78167

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.