MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aardvark Polymers Aarlon® 4055FR PA 6/6 Rotational Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes:
  • Aarlon 4055FR is a premium flame retardant type 6/6 nylon.
  • Aarlon 4055FR is halogen, heavy metal, and red phosphorus free.
  • Aarlon 4055FR is UL94 V-0 rated.
  • Aarlon 4055FR is semi-crystalline, nucleated, and heat stabilized.
  • Aarlon 4055FR is available in natural and may be colored and/or printed.
  • Aarlon 4055FR is applicable for industrial markets such as automotive, aerospace, and electronics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccDAM
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 1.57 mm
DAM
 0.011 cm/cm
@Thickness 3.17 mm
DAM
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 1.60 mm
DAM
 0.011 cm/cm
@Thickness 3.20 mm
DAM
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 89.2 MPaDAM
Elongation at Break 14 %DAM
Flexural Modulus 3.43 GPaDAM
Izod Impact, Unnotched 0.430 J/cmDAM
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CDAM
Deflection Temperature at 0.46 MPa (66 psi) 230 °CDAM
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CDAM
UL RTI, Electrical 130 °C
@Thickness 1.50 mm
DAM
 130 °C
@Thickness 3.00 mm
DAM
UL RTI, Mechanical with Impact 75.0 °C
@Thickness 1.50 mm
DAM
 75.0 °C
@Thickness 3.00 mm
DAM
UL RTI, Mechanical without Impact 85.0 °C
@Thickness 1.50 mm
DAM
 85.0 °C
@Thickness 3.00 mm
DAM
Flammability, UL94 V-0
@Thickness 0.800 mm
DAM, Test 1
 V-0
@Thickness 0.800 mm
DAM, Test 2
 V-0
@Thickness 1.50 mm
DAM, Test 1
 V-0
@Thickness 1.50 mm
DAM, Test 2
 V-0
@Thickness 3.00 mm
DAM, Test 1
 V-0
@Thickness 3.00 mm
DAM, Test 2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Toyobo GLAMIDE® T-662 Nylon-66
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6)

PGAPOLZ0 / 39216

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.