MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Novatec Novaloy® 9000 PVC + ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/PVC Alloy; Vinyl (PVC)

Material Notes: Novaloy® 9000 is a specialty engineering alloy of ABS/PVC designed for injection molding, profile and sheet extrusion. Novaloy® 9000 has been formulated to provide excellent processing characteristics, high heat distortion temperatures along with excellent retention of physical properties upon aging. Impact resistance is excellent at both room and low temperature. Raw material appearance is Colored Opaque Pellets.

Applications: Products made from Novaloy® 9000 are suitable for a variety of applications such as appliance housings, electrical boxes, communications, lawn and garden applications as well as recreational.

Information supplied by the manufacturer.

PolyOne (Avient) acquired the Novatec polymer resin product line. This grade is not a part of their current product line

Key Words: Excellent processing characteristics, high heat distortion temperatures, excellent aging
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 - 1.23 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 42.2 MPaASTM D638
Modulus of Elasticity 2.41 GPaASTM D638
Flexural Yield Strength 75.2 MPaASTM D790
Flexural Modulus 2.41 GPaASTM D790
Izod Impact, Notched 4.00 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 76.9 °CASTM D648
Oxygen Index 31 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman ComAlloy Comtuf® 522 Polycarbonate/Styrenic Alloy
Overview of materials for ABS/PVC Alloy
Spartech Royalite R59M Hi-Impact ABS/PVC Resin
Spartech Royalite R60M Hi-Impact ABS/PVC Resin
Lotte Advanced Materials Starex® WR-9100 ASA, Unreinforced

PNV100 / 55511

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.