MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Bicor™ 21MB621 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both sides. The static resistant feature of this film prevents the attraction of dust, and contributes to excellent machine performance even on critical packaging machines. The acrylic coating is water based and provides wide heat sealing range on packaging equipment.

Availability: Africa & Middle East, Asia Pacific and Europe

Key Features:

  • Low sealing threshold
  • Efficient Sealability under Low Pressure
  • Optimum and Stable Coefficient of Friction
  • Excellent Performance on Overwrap Packaging Machines
  • Outstanding Optical Properties
  • Good Aroma Barrier
  • Ideal Support for Normal Ink Systems
  • Water Based Coatings
Features:
  • Acrylic Coated
  • Flavor & Aroma Barrier
Applications:
  • Box Overwrap
  • Confectionery, Chocolate
  • Confectionery, Gum
  • Confectionery, Sugar
  • Health and Beauty Care
Uses:
  • Box Overwrap Flexible Packaging
Processing Method: Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print Unsupported

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 0.0900 g/100 in²/day
@Temperature 23.0 °C
85% RH; ExxonMobil Method
 0.450 g/100 in²/day
@Temperature 38.0 °C
90% RH; ExxonMobil Method
Thickness 0.830 milExxonMobil Method
Coating Weight 11.7 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 140 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 50 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 319 ksiMD; ExxonMobil Method
 580 ksiTD; ExxonMobil Method
Coefficient of Friction 0.25Both Sides; ExxonMobil Method
Seal Strength 200 g/in
@Pressure 0.00345 MPa,
Temperature 100 °C
0.5 sec, LPS; ExxonMobl Method
 510 g/in
@Pressure 0.276 MPa,
Temperature 140 °C
Otto Bruger, 0.2 sec; ExxonMobl Method
Film Tensile Strength at Break, MD 18900 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 36300 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 5.0 %
@Temperature 135 °C,
Time 432 sec
ExxonMobil Method
Shrinkage, TD 3.0 %
@Temperature 135 °C,
Time 432 sec
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %ExxonMobil Method
Gloss 85 %45°; ExxonMobil Method
 
Descriptive Properties
Heat Seal Range72°F36.3 psi, 0.2 sec
Yield36800 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Bicor™ 18MB090 OPP Film
ExxonMobil Bicor™ 30MBR666 OPP Film
ExxonMobil Bicor™ 25 ARW OPP Film
ExxonMobil Metallyte™ UHB 35MU842 OPP Film
ExxonMobil Metallyte™ 28UBW-ES OPP Film

PEX99469 / 175705

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.