System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Arnitel® VT3108 TPC-ET
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyester TPE
;
Polyester, TP
Material Notes:
Extrusion Grade, High Breathable, Drying of Material Required
Former DSM Engineering Plastics product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.25
g/cc
ISO 1183
Melt Flow
10
g/10 min
@Load 2.16 kg,
Temperature 230 °C
cm
3
/10min Melt Volume-flow Rate; ISO 1133
Mechanical Properties
Original Value
Comments
Hardness, Shore D
45
@Time 3.00 sec
ISO 868
Tensile Strength, Ultimate
20.0
MPa
ISO 527-1/-2
Tensile Stress at Strain
5.10
MPa
@Strain 5.0 %
ISO 527-1/-2
8.10
MPa
@Strain 10 %
ISO 527-1/-2
12.5
MPa
@Strain 50 %
ISO 527-1/-2
14.1
MPa
@Strain 100 %
ISO 527-1/-2
Elongation at Break
280 %
ISO 527-1/-2
Tensile Modulus
0.110
GPa
ISO 527-1/-2
Izod Impact Resistance
NB
@Temperature 23.0 °C
ISO 180/1A
NB
@Temperature -30.0 °C
ISO 180/1A
Charpy Impact, Notched
NB
@Temperature 23.0 °C
ISO 179/1eA
NB
@Temperature -30.0 °C
ISO 179/1eA
Thermal Properties
Original Value
Comments
Melting Point
185
°C
10°C/min; ISO 11357-1/-3
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Envalior Arnitel® PL380 TPC-ET, Injection Molding
Envalior Stanyl® Diablo OCD2100 BK27021 PA46-GF40, Dry, 40% Glass Filled, Heat Stabilized
Envalior Arnitel® EM400 TPC-ET, Injection Molding or Extrusion Grade
Envalior Arnitel® PL381 TPC-ET, Injection Molding
Envalior Arnitel® PM471 TPC-ET, Injection Molding
PDSM9805 / 161426
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.