MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Albis Plastics Polypropylene PP 14A3 GF15 C , 15% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Semi-crystalline Polypropylene Copolymer (PPCP)

Characteristics: Chemically Coupled: Good Strength and Stiffness

Applications: Appliances, Furniture, Cases, Packaging and Novelties

Processing: Injection Molding (Melt Temperature: 430-575°F, Mold Temperature: 70-160°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cmASTM D955
Melt Flow 3.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 47.6 MPaASTM D638
Elongation at Break 5.7 %ASTM D638
Flexural Yield Strength 55.2 MPaASTM D790
Flexural Modulus 1.93 GPaASTM D790
Izod Impact, Notched 1.17 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CASTM D648
Vicat Softening Point 93.0 °C(VST/B/120); ASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 221 - 302 °CInjection
Mold Temperature 21.0 - 71.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES HiFill® PP GF15 CC 15% Glass Filled
Techmer ES HiFill® PP CO GF15 CC 15% Glass Filled
A. Schulman Diamond NPP25-0120B GF15 Glass Filled Copolymer Polypropylene
Polykemi AB POLYfill PPH DGF101015 PB Polypropylene Homopolymer, Glass Fibre/Mineral, Chemically Coupled
Polykemi AB POLYfill PPC GF15030 PD2 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled

PZA1B90 / 21777

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.