MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Old Hickory 44-B Kentucky Ball Clay  (discontinued **)
Categories: Ceramic; Clay; Ball Clay

Material Notes: The 44-B clay is similar to 54-S and is a recommended selection where additional plasticity and strength are important. It is particularly recommended in extruded and plastic processed ceramic formulas such as electrical porcelain and tableware. The 44-B can also be used in monoporosa and monocuttura tile bodies for additional press density and strength especially for a large dimension shapes.

Information provided by Old Hickory Clay Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 0.45 µmMedian particle diameter
 0.50 µm52% of particles less than
 1.0 µm62% of particles less than
 <= 5.0 µm83% of particles less than
pH 6.3
Soluble Sulfates 520 ppm
Specific Surface Area 19.2 m²/g
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.650 ksiDry Modulus of Rupture for 50% clay/50% flint, cast bars
 
Thermal PropertiesOriginal ValueComments
Shrinkage 5.0 %Cone 04, Linear Fired Shrinkage
 5.8 %Cone 3, Linear Fired Shrinkage
 6.3 %Linear Drying Shrinkage
 6.7 %Cone 11, Linear Fired Shrinkage
 
Component Elements PropertiesOriginal ValueComments
Al2O3 28.5 %
CaO 0.15 %
Fe2O3 1.15 %
K2O 1.22 %
Loss on Ignition(%) 9.5 %
MgO 0.16 %
Na2O 0.10 %
SiO2 57.7 %
TiO2 1.52 %
 
Descriptive Properties
Absorption (%)10.1Cone 04, Fired
 3.5Cone 11, Fired
 8.6Cone 3, Fired
CEC/MBI (meg/100 ml)10
Crude ColorLight Grey
Filtration (ml)19
Pyrometric Cone Equivalent (PCE)29-31
Water of Plasticity (%)33
Wet Sieve Residue (%)0.8Wet Sieve Residue, +200 mesh

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mo-Sci Corporation GL 0179 Borosilicate glass frit
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Titanium Grade 2
Plaster; Molded, Dry
Old Hickory No. 6 Kentucky Ball Clay

EOHC901 / 161980

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.