MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® HTplus F1001 Polyphthalamide  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: VESTAMID HTplus F1001 is based on a polyphthalamide (PPA). This special resin is specifically tailored for manufacturing monofilaments which can be subjected to high temperature. VESTAMID HTplus F1001 is supplied as spherical pellets in polyethylene packaging. Drying at 120°C for at least 4 hours before processing is recommended. For information about processing of VESTAMID HTplus, please follow the general recommendations for PPA in our brochure „Handling and Processing of VESTAMID HTplus.“

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaISO 527-1
 >= 300 MPaAfter extrusion; ISO 527-1
 >= 300 MPaafter conditioning (3h/180°C); ISO 527-1
Elongation at Break 3.0 %ISO 527-1
 >= 150 %After extrusion; ISO 527-1
 >= 150 %after conditioning (3h/180°C); ISO 527-1
Tensile Modulus 3700 MPaISO 527-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 300 - 315 °CISO 11357

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAMID® HTplus M1031 Polyphthalamide
Evonik VESTAMID® HTplus C2505 PA10T/X
Evonik VESTAMID® HTplus M1054 PA6T/X, MD40
Evonik VESTAMID® HTplus F2001 PA10T/X
Evonik VESTAMID® HTplus LDS3031 PA10T/X, GF10

PEVONIL237 / 196441

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.