MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Wacker Silpuran® 8020/60 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product description: SILPURAN® 8020/60 is an addition-cure, two-component high consistency silicone rubber for the manufacture of molded articles. The vulcanizates show an excellent transparency and good to very good mechanical properties.

Special features: SILPURAN® 8020/60 is packaged in accordance with class 8 clean room standards (DIN EN ISO 14644). SILPURAN® 8020/60 meets selected test requirements of ISO 10993 and United States Pharmacopoeia (USP) Class VI. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Application: SILPURAN® 8020/60 is particularly suitable for the economical production of molded articles by compression, transfer or injection molding. SILPURAN® 8020/60 is designed for medical applications including implantation for < 30 days.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/cc
@Pressure 0.1013 MPa
DIN 53479
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60DIN 53505
Tensile Strength at Break 11.2 MPaDIN 53505 S1
Elongation at Break 670 %DIN 53505 S1
Rebound 57 %DIN 53512
Tear Strength 31.0 kN/mASTM D624B
Compression Set 30 %
@Temperature 175 °C,
Time 79200 sec
DIN ISO 815-B
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Treatment Temp. 165 °C
postcuring for 4 h/200 °C in ventilated air.
 15.0 min
@Treatment Temp. 165 °C
postcuring for 6 h/200 °C in ventilated air.
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Colortransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® R 701/60 Silicone Rubber
Shin-Etsu Silicones KE-9611U Silicone Elastomer
Precision Polymer Engineering S60R Silicone Rubber
Elkem (Bluestar Silicones) SILBIONE® HCRA 4150 A/B HC Silicone Rubber
Dow Silastic® LC-50-2004 PART A&B KIT

PWACK9509 / 205038

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.