MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
C.O.I.M. LARIPUR® LPR5450 Modified Ester Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyester Thermoplastic Elastomer; Polyurethane, TP

Material Notes: Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:
  • Excellent abrasion resistance
  • Great flexibility with constancy at temperature variations
  • Good compression resistance
  • Good water and light resistance
  • Good resistance to oils, fats and to many types of solvents

Series 50 Modified Ester: These products are obtained by homogeneously incorporating a small amount of raw material of unique chemical composition to the products of Series 25. They combine a high level of hardness with excellent cold impact resistance.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 53ASTM D2240
Tensile Strength, Yield 60.8 MPaASTM D412
Elongation at Break 450 %ASTM D412
50% Modulus 0.0116 GPa
@Strain 50 %
ASTM D412
100% Modulus 0.0141 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0364 GPa
@Strain 300 %
ASTM D412
Flexural Modulus 0.159 GPaASTM D790
Tear Strength 150 kN/mASTM D624
Abrasion 40mm3, Abrasion Loss; DIN 53516
Torsional Stiffness 37.0 MPa+20°C; ASTM D1043
 170 MPa-20°C; ASTM D1043
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 104 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR8020 Standard Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR5520 Standard Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR5850 Modified Ester Polyurethane
C.O.I.M. LARIPUR® LPR9020 Standard Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR6515 Plasticized Ester Polyurethane

PCOIM016 / 28619

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.