MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nylene® 826 Nylon Copolymer
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Dry as molded. Nylene 826 is a special nylon copolymer suitable for both blown and cast film co-extrusion. Nylene 826 has a lower melt point and is less crystalline than standard nylon 6 resins. In addition to excellent toughness, chemical resistance, transparency, and low oxygen permeability, films exhibit superior deep-drawing characteristics. Effective processing is achieved with extruder and die temperatures in the range of 450 - 525ºF.

ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.

Key Words: Polyamide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPaASTM D638
Elongation at Break 365 %ASTM D638
 
Processing PropertiesOriginal ValueComments
Processing Temperature 232 - 272 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® C33 01 PA66/6 (Dry)
Nylene® CX3395 Nylon Copolymer
BASF Ultramid® KR 4350 PA6/6T (Conditioned)
Avient Bergamid™ AB700 UF Polyamide 66/6 Copolymer (Nylon 66/6)
BASF Ultramid® C33 01 PA66/6 (Conditioned)

PN6C5I / 54252

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.