MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® 2851FT One-Component Thermally Conductive Encapsulant
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Provides excellent heat dissipation and thermal shock resistance as well as protection from moisture and chemical agents. Typical applications include sensors, transformers, transducers, switches, and other small devices.
  • Excellent Chemical Resistance
  • Filled
  • High temperature
Cure Type: Heat Bonding Type: Epoxy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.30 g/ccUncured
Water Absorption 0.060 %
@Time 86400 sec
Immersion
Viscosity 85000 cPUncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 90
Tensile Strength 50.0 MPa
Flexural Strength 93.0 MPa
Compressive Strength 130 MPa
Izod Impact, Notched 0.160 J/cm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
Dielectric Constant 5.2
@Frequency 1e+6 Hz
Dissipation Factor 0.020
@Frequency 1e+6 Hz
Arc Resistance 207 sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µm/m-°C
Thermal Conductivity 1.36 W/m-K
Heat Distortion Temperature 102 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 120 °C
Option 1, A post cure of 4 hours @ 150°C is recommended.
 2.00 hour
@Temperature 110 °C
Option 2, A post cure of 4 hours @ 150°C will improve final end-properties.
 5.00 hour
@Temperature 90.0 °C
Option 3, A post cure of 4 hours @ 150°C will improve final end-properties.
Shelf Life 6.00 Month
@Temperature 0.000 - 8.00 °C
From date of manufacture

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Stycast® 2760 Two-Component Easy Mix Ratio Encapsulant
Trelleborg Emerson & Cuming Stycast® 2072 Two-Component Easy Mix Ratio Encapsulant
Trelleborg Emerson & Cuming Stycast® E-1000 One-Component Epoxy Low Stress Encapsulant
Trelleborg Emerson & Cuming Stycast® E-151-8 One-Component Epoxy Flexible Encapsulant
Henkel Loctite® Stycast® 2850FT/11 Two-Component Thermally Conductive Encapsulant

PEMERS38 / 35730

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.