MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Menzolit Menzolit® BMC 1400 Unsaturated Polyester UP
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: BMC 1400 is a special BMC for the use on an engine. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The product has been developped fot high resistance against gasoline, lubricants, cooling agents or cleaning agents that are used around an automotive engine. Because of its resin matrix it is especially resistant to cyclic loads under elevated temperature. Typical applications are valve covers, gear box covers, carburator housings, or housings for auxiliary motors.

Information Provided by Menzolit

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³ISO 1183
Water Absorption <= 0.30 %<= 0.30 %ISO 62
Linear Mold Shrinkage 0.00030 cm/cm0.00030 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 37.0 MPa
@Temperature 22.0 °C
5370 psi
@Temperature 71.6 °F
25 mm flat samples, compression molded; ISO 527-4
Tensile Strength, Yield 37.0 MPa
@Temperature 22.0 °C
5370 psi
@Temperature 71.6 °F
25 mm flat samples, compression molded; ISO 527-4
Elongation at Break 0.00 %0.00 %ISO 527-4
Modulus of Elasticity 13.0 GPa1890 ksi25 mm flat samples, compression molded; ISO 527-4
Flexural Strength 125 MPa
@Temperature 22.0 °C
18100 psi
@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Flexural Modulus 10.0 GPa
@Temperature 22.0 °C
1450 ksi
@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Poissons Ratio 0.300.30
Shear Modulus 5.00 GPa725 ksiin plane
Charpy Impact, Notched 3.50 J/cm²16.7 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 4.04.0IEC 60250
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243-1
Dissipation Factor 0.0100.010IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 µm/m-°C5.56 µin/in-°FISO 11359-2
Specific Heat Capacity 1.10 J/g-°C0.263 BTU/lb-°F
Thermal Conductivity 0.700 W/m-K4.86 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 170 °C338 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 150 °C>= 302 °FISO 75-2
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 162 °C324 °FISO 11357-2
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Oxygen Index 22 %22 %ISO 4589-2
Glow Wire Flammability Index 750 °C1380 °FIEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 135 - 160 °C275 - 320 °FInjection molding, matched metal die

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vyncolit X655RB Glass Fiber and Mineral Filled Novolac Phenolic
Menzolit Menzolit® BMC 3100 Unsaturated Polyester UP
Bakelite® PF 6510 Phenolic Molding Compound

PMENZ014 / 100748

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.