MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-17365 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-17365 is a high performance thermoplastic elastomer, available in NAT and colors, specifically designed for healthcare and medical applications. Medalist MD-17365 is a medium hardness, low density, halogen-free grade that can be sterilized and is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Colorability; Good Flexibility; Good Moldability; Halogen Free; Low Density; Low Flow; Medium Hardness; Low Specific Gravity; Radiation (Gamma) Resistant; Radiation Sterilizable; Resilient; Slip; Without Fillers

Uses: Bladders; Bushings; Connectors; Disposable Hospital Goods; Flexible Grips; Grommets; Handles; Knobs; Medical/Healthcare Applications; Pharmaceuticals; Plugs; Rubber Replacement; Seals

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccASTM D792
Melt Flow 2.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 66
@Time 5.00 sec
Injection Molded; ASTM D2240
 68
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 1700 psiASTM D412
Tensile Stress at Strain 360 psi
@Strain 100 %
ASTM D412
 650 psi
@Strain 300 %
ASTM D412
Elongation at Break 750 %ASTM D412
Compression Set 16 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 84 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Processing Temperature 340 - 380 °FMelt, Injection
Rear Barrel Temperature 260 - 300 °FInjection
Middle Barrel Temperature 280 - 320 °FInjection
Front Barrel Temperature 300 - 340 °FInjection
Nozzle Temperature 340 - 380 °FInjection
Zone 1 280 - 300 °FExtrusion
Zone 2 300 - 320 °FExtrusion
Zone 3 320 - 360 °FExtrusion
Zone 4 320 - 360 °FExtrusion
Zone 5 340 - 380 °FExtrusion
Die Temperature 360 - 400 °FExtrusion
Mold Temperature 70.0 - 100 °FInjection
Injection Pressure 200 - 800 psi
Back Pressure 25.0 - 100 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-12362 Thermoplastic Elastomer
Teknor Apex Medalist® MD-12160H Thermoplastic Elastomer
Teknor Apex Medalist® MD-32265 Thermoplastic Elastomer
Teknor Apex Medalist® MD-17270 Thermoplastic Elastomer
Teknor Apex Medalist® MD-50357 Thermoplastic Elastomer

PTEKNQ0713 / 237204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.