MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
A. Schulman BMC 940 Vinyl Ester Bipolar Plate Material
Categories: Polymer; Thermoset; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most cost-effective plastic products on the market today. The process of manufacturing BMC thermosets is geared toward high-volume, automated systems to ensure the highest quality at the lowest possible cost. BMC thermosets can be designed to conduct electricity for use in applications such as bipolar plates that are used in fuel cells.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.82 g/ccASTM D792
Water Absorption <= 0.060 %24 hours, 23°C; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 4400 psiASTM D638
Flexural Strength >= 5800 psiASTM D790
Flexural Modulus >= 1500 ksiASTM D790
Izod Impact, Unnotched 0.300 ft-lb/in
Dynatup @ -18°C 2.63 ft-lb
Dynatup @ -18°C Max Load 169 lb
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.010 ohm-cmin plane
 0.020 ohm-cmThrough plane
 
Thermal PropertiesOriginal ValueComments
CTE, linear >= 30.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.841 J/g-°Cthrough-plane
Thermal Conductivity 19.2 W/m-KThrough Plane
 46.2 W/m-KIn-Plane
 18.5 W/m-K
@Temperature 85.0 °C
Through Plane
 43.7 W/m-K
@Temperature 85.0 °C
In Plane
Glass Transition Temp, Tg >= 200 °C
Flammability, UL94 V-0
@Thickness 3.56 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 325 - 335 °F
Cure Time 30.0 - 60.0 sec
 
Descriptive Properties
Compressive Creep, 200 psi0.025%200hr @ 80°C
 0.04%1000hr @ 80°C
Diffusivity, cm²/s0.09885°C Through Plane
 0.12525°C Through Plane
 0.23185° In-Plane
 0.30225° In-Plane
DMA-Modulus0.510^6 psi, 200°C
 0.9410^6 psi, 175°C
 1.2310^6 psi, 150°C
 1.610^6 psi, 100°C
 210^6 psi, 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC 845 30% Glass Filled Vinyl Ester
A. Schulman BMC 845 Vinyl Ester Molding Compounds, 30% Glass-Filled
A. Schulman BMC 695 Vinyl Ester Molding Compound
Quantum Composites QC-8805 66% Glass Fiber Vinyl Ester SMC
Haysite 24500 Vinyl Ester BMC, 20% Glass Reinforced

PBMC069 / 27252

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.