MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Silfoam® SE 23 FOOD GRADE Silicone Antifoam Emulsion
Categories: Fluid

Material Notes: Product description: SILFOAM® SE23 FOOD GRADE is a 30% active emulsion designed for controlling foam in aqueous systems. SILFOAM® SE23 FOOD GRADE contains those ingredients which are suitable per the FDA requirements as published in the CODE OF FEDERAL REGULATIONS. (Under Title 21 "Food and Drugs," Part 173, "Secondary Direct Food Additives Permitted in Food for Human Consumption," Paragraph 173.340 "Defoaming Agents"). Because this regulation contains limitations, compliance to the regulation is the responsibility of the manufacturer of the finished product. SILFOAM® SE23 FOOD GRADE is also suitable for other food contact applications. SILFOAM® SE23 FOOD GRADE is registered by NSF to Category Code 3D (as a fruit and vegetable washing product) and Q5 (for use as foam control agent in egg washing machines). SILFOAM® SE23 FOOD GRADE is suitable for use in secondary or indirect food contact applications listed under FDA 21 CFR176.170; 176.180; 176.200; 176.210;175.300; 177.2600; and178.3400. SILFOAM® SE23 FOOD GRADE can also be used in various industrial foam control applications and as a dispersion/coating leveling agent

Special features:

  • Long lasting foam control
  • Rapid foam knockdown
  • Chemically stable
  • No offensive odor
Application: SILFOAM® SE23 FOOD GRADE can be added easily to most foaming systems as is or by diluting with either water or a portion of the foaming system. In hot systems and in processes where maximum uniformity of the dispersion is required, SILFOAM® SE23 FOOD GRADE is best diluted with cool water before adding it to the foaming solution. Prior to use, SILFOAM® SE23 FOOD GRADE should be gently stirred with minimum shear to assure uniformity of the emulsion.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/cc
pH 4.3
Viscosity 3000 - 15000 cP
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Active ingredients (%)33
Appearancewhite, creamy liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow XIAMETER® PMCPPMX-200 350CS Food Grade Silicone Fluid
Wacker Wacker® AK 350 Food Grade/Kosher Silicone Fluid
Wacker Wacker® AK 1000 US Food Grade/Kosher Silicone Fluid
Wacker Silfoam® SE 21 FOOD GRADE Silicone Antifoam Emulsion
Wacker Silfoam® SC 203 FOOD GRADE Silicone Antifoam Compound

PWACK9455 / 204984

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.