MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
UPM Formi Formi SP 50 50% Cellulose Fiber Reinforced Polypropylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Wood Filled

Material Notes: Material: UPM Formi is a cellulose fiber reinforced plastic composite with high renewable material content. It is specially designed for injection molding applications. Principal ingredients are specially selected cellulose fibers and virgin polypropylene. Cellulose fibers significantly increase stiffness and strength of polypropylene

Applications: Environmentally sound UPM Formi composite can be used in injection molding applications instead of polypropylene, filled polypropylene or several other plastics

Environment: UPM Formi is manufactured from renewable cellulose fibers which reduce usage of oil based plastics. Material is fully recyclable or can be burned for energy. All cellulose fibers are from sustainably managed forests.

Information provided by UPM

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 66.0 MPa50 mm/min; ISO 527-2
Elongation at Break 3.5 %50 mm/min; ISO 527-2
Tensile Modulus 5500 MPa1 mm/min; ISO 527-2
Charpy Impact Unnotched 37.0 kJ/m²ISO 179-2/1eU
Charpy Impact, Notched 7.00 kJ/m²ISO 179-2/1eA
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 200 °C
Mold Temperature 60.0 - 120 °C
Drying Temperature 115 °C
Dry Time 3.00 hour
Injection Pressure <= 120 MPa
 
Descriptive Properties
Temperature profile from nozzle190/185/180/175 ºC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PUPMF005 / 286813

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.