System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Celanese Celanex® 6500HR PBT, Mineral / Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Material Notes:
6500HR is a hydrolysis resistant, 30% glass/mineral filled polyester with improved warp resistance and surface smoothness.
Information provided by Celanese Corporation.
Key Words:
30% glass/mineral filled polyester, low warp, hydrolysis resistant.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.55
g/cc
ASTM D792
Density
1.555
g/cc
ISO 1183
Moisture Absorption at Equilibrium
0.19 %
23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow
0.0020
-
0.0050
cm/cm
ISO 294-4
Linear Mold Shrinkage, Transverse
0.00
-
0.0050
cm/cm
ISO 294-4
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
91
ISO 2039-2
Tensile Strength at Break
125
MPa
5mm/min; ISO 527-2/1A
16000
psi
@Temperature 22.8 °C
ASTM D638
Elongation at Break
2.2 %
5mm/min; ISO 527-2/1A
3.0 %
@Temperature 22.8 °C
ASTM D638
Tensile Modulus
9700
MPa
1mm/min; ISO 527-2/1A
Flexural Strength
180
MPa
ISO 178
28000
psi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus
9500
MPa
ISO 178
1.35e+6
psi
@Temperature 22.8 °C
ASTM D790
Izod Impact, Notched
1.40
ft-lb/in
@Temperature 22.8 °C
ASTM D256
Izod Impact, Notched (ISO)
5.30
kJ/m²
ISO 180/1A
Charpy Impact Unnotched
26.0
kJ/m²
ISO 179/1eU
23.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched
5.90
kJ/m²
ISO 179/1eA
6.30
kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+14
ohm-cm
IEC 60093
1.00e+17
ohm-cm
ASTM D257
Surface Resistance
2.00e+16
ohm
IEC 60093
Dielectric Constant
3.0
@Frequency 100 Hz
IEC 60250
3.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength
19.0
kV/mm
IEC 60243-1
600
V/mil
short term; ASTM D149
Dissipation Factor
0.017
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
275
V
IEC 60112
Thermal Properties
Original Value
Comments
Melting Point
225
°C
ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi)
223
°C
ISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi)
202
°C
ISO 75-1, -2
Glass Transition Temp, Tg
54.0
°C
ISO 11357-1,-2,-3
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PHCS093 / 123508
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.