System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
RheTech Products HP510-01UV 28% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 30% Talc Filler
Material Notes:
Applications:
Air ducts-structural
Interior trim
I/P components
Center consoles
Injection molding conditions reported in table.
Information provided by RheTech Products.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.11
g/cc
@Temperature 23.0 °C
23/23°C; ASTM D792
Filler Content
28 %
ASTM D5630
Linear Mold Shrinkage
0.0119
cm/cm
ASTM D955
Melt Flow
6.0
g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore D
73
ASTM D2240
Tensile Strength at Break
4200
psi
2 in/min; ASTM D638
Flexural Modulus
380000
psi
Tangent; ASTM D790
Izod Impact, Notched
0.600
ft-lb/in
@Temperature 23.0 °C
ASTM D256
Gardner Impact
0.830
ft-lb
ASTM D5420
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
250
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
170
°F
ASTM D648
Processing Properties
Original Value
Comments
Rear Barrel Temperature
400
-
450
°F
Middle Barrel Temperature
410
-
460
°F
Front Barrel Temperature
420
-
470
°F
Nozzle Temperature
430
-
450
°F
Mold Temperature
80.0
-
120
°F
Drying Temperature
150
-
180
°F
Dry Time
1
-
2
hour
Moisture Content
<= 0.050 %
Recommended
Injection Pressure
400
-
1500
psi
Hold Pressure
300
-
1200
psi
Back Pressure
50.0
-
150
psi
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Phillips Sumika Marlex® CHP-260 Polypropylene Compound, Engineered TPO, high-impact resin
RheTech Products HP506-01 20% Talc Reinforced High Performance Polypropylene, Black
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black
RheTech Products F24-01 20% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
PRHET207 / 65775
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.