MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATG s.r.l. FPM Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.82 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50 - 90
Tensile Strength, Ultimate 5.00 - 17.0 MPa
Elongation at Break 125 - 300 %
Rebound 5.0 - 10 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °C
Minimum Service Temperature, Air -20.0 °C
 
Descriptive Properties
Abrasion Resistancemedium
Chemical Resistance to Animal and Vegetable Oils and Greaseshigh
Chemical Resistance to Aromatic Hydrocarbonshigh
Chemical Resistance to Chloride Solventshigh
Chemical Resistance to Distilled Watermedium
Chemical Resistance to Ketonesnone
Chemical Resistance to Maximum Concentrated Alkalis (at 50°C)low
Chemical Resistance to Medium-High Concentrated Acids (at 50°C)medium
Chemical Resistance to Mineral Oils and Aliphatic Hydrocarbonshigh
Compression set at 100°Chigh
Impermeability at gas (Oxygen and Nitrogen)high
Resistance to Flamehigh
Resistance to Heat Aginghigh
Resistance to Low Temperatureslow
Resistance to Ozone and Weatheringhigh
Tear Strengthmedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fluorocarbon Rubber (FPM), Low Temperature Grade
Tipco Tipcolene® FPM 40 - 40% Mica Reinforced Polypropylene Homopolymer, High Stiffness
Ethylene Propylene Rubber (EPM, EPDM)
Momentive Performance Materials RTV88 Red Extreme High Temperature Potting/Encapsulating Compound
ATG s.r.l. EPDM Ethylene-Propylene Terpolymer

PATG020 / 79385

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.