MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nabaltec APYRAL® 40 VS1 Al(OH)3
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: The high quality and performance of our surface treated APYRAL® 40VS1 and APYRAL® 60VS1 powders complete the APRYAL® product range for highly specialized applications. Examples include, excellent tracking resistance in electronics and extreme low water absorption of HFFR cable compounds, where vinylsilane modified APYRAL® products are almost indispensable.

APYRAL ® can be used as a flame retardant filler in

  • Thermosets
  • Elastomers
  • Thermoplastics
  • Cable Compounds
  • Technical Rubber Compounds
  • Pressed and cast Plastic Parts
  • Thermal Insulation Foams
  • Glass-fiber reinforced plastics

Key Words: Aluminum Hydroxide, Al(OH)3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.350 g/cc
Density 2.40 g/cc
Brightness 91 %
@Wavelength 457 nm
Whiteness; Elrepho
Oil Absorption 33 %ml/100 g
Moisture Absorption at Equilibrium 0.20 %
Loss On Ignition 34.6 %
@Temperature 105 - 1000 °C
Particle Size 1.5 µmMedian Grain Diameter
Specific Surface Area 3.5 m²/gBET
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 33333 ohm-cm
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.58
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 0.010 %
Na2O 0.20 %
SiO2 0.30 %
 
Descriptive Properties
Al(OH)3 wt %98.5
Mechanical Properties as AdditiveElongation at break: 240 %
 Tensile Strength: 14 MpaHFFR-EVA cable compound
Sieve Analysis (%)0.05> 45 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nabaltec APYRAL® 60CD Al(OH)3
Nabaltec APYRAL® 40CD Al(OH)3
Nabaltec APYRAL® 120E Al(OH)3
Arkema EVATANE® 28-05 Copolymer Ethylene - Vinyl Acetate
Silberline Sparkle Silvet® 880-20-J

CNABAL17 / 54542

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.