Mechanical Properties | Original Value | Comments |
---|
Tensile Strength | 12100 psi @Temperature 82.0 °C |
| 33700 psi @Temperature 104 °C |
| 37900 psi @Temperature 104 °C |
| 38800 psi @Temperature 82.0 °C |
| 55900 psi @Temperature 104 °C |
| 66300 psi @Temperature 22.0 °C |
| 68500 psi @Temperature 22.0 °C |
| 78000 psi @Temperature -54.0 °C |
| 92200 psi @Temperature -54.0 °C |
Elongation at Break | 1.52 % @Temperature 104 °C |
| 1.55 % @Temperature -54.0 °C |
Tensile Modulus | 21.6 GPa @Temperature 104 °C |
| 21.9 GPa @Temperature 104 °C |
| 23.6 GPa @Temperature 82.0 °C |
| 25.3 GPa @Temperature 104 °C |
| 26.3 GPa @Temperature 22.0 °C |
| 26.4 GPa @Temperature 82.0 °C |
| 27.0 GPa @Temperature 22.0 °C |
| 27.0 GPa @Temperature -54.0 °C |
| 28.1 GPa @Temperature -54.0 °C |
Compressive Strength | 166 MPa @Temperature 104 °C |
| 197 MPa @Temperature 104 °C |
| 260 MPa @Temperature 82.0 °C |
| 312 MPa @Temperature 82.0 °C |
| 483 MPa @Temperature 22.0 °C |
| 517 MPa @Temperature 104 °C |
| 563 MPa @Temperature -54.0 °C |
| 629 MPa @Temperature 22.0 °C |
| 786 MPa @Temperature -54.0 °C |
Compressive Modulus | 25000 MPa @Temperature 82.0 °C |
| 26600 MPa @Temperature 82.0 °C |
| 27700 MPa @Temperature 82.0 °C |
| 28000 MPa @Temperature 82.0 °C |
| 28000 MPa @Temperature 22.0 °C |
| 29000 MPa @Temperature 22.0 °C |
| 29000 MPa @Temperature -54.0 °C |
| 29400 MPa @Temperature 22.0 °C |
| 29700 MPa @Temperature 22.0 °C |
| 30000 MPa @Temperature -54.0 °C |
| 30300 MPa @Temperature -54.0 °C |
| 30300 MPa @Temperature -54.0 °C |
Shear Modulus | 1.50 GPa @Temperature 104 °C |
| 2.70 GPa @Temperature 82.0 °C |
| 5.00 GPa @Temperature 22.0 °C |
| 6.30 GPa @Temperature -54.0 °C |
| 24.0 GPa @Temperature 121 °C |
| 26.0 GPa @Temperature 22.0 °C |
Shear Strength | 7600 psi @Temperature 104 °C |
| 8600 psi @Temperature 82.0 °C |
| 14500 psi @Temperature 22.0 °C |
| 19000 psi @Temperature -54.0 °C |
| 86000 psi @Temperature 121 °C |
| 100000 psi @Temperature 22.0 °C |
|
Thermal Properties | Original Value | Comments |
---|
Maximum Service Temperature, Air | 220 °F |
|
Processing Properties | Original Value | Comments |
---|
Gel Time | 5.00 - 8.00 min @Temperature 121 °C |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to go back to viewing the property data in MatWeb's normal format.