MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Indium Corp. Sn995 Cobalt-Doped, Pb-Free Soldering Alloy
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: Sn995 Cobalt-Doped Pb-Free Soldering Alloy is a cobalt-doped Sn/Cu alloy that provides a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn/Cu alloy produces smoother, shinier joints and lower dross than SAC305 and other Sn/Cu based alloys

Features

  • Shiny, smooth solder joints similar to Sn/Pb solder
  • Low cost - does not contain Ag
  • Lower dross formation than other SAC and Sn/Cu-based alloys
  • Less copper erosion than SAC305
  • Compatible with other Sn/Cu-based alloys - no need to dump the pot
  • Available in a solder bar for wave soldering and cored wire for rework applications

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 28.0 MPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 228 °C
 
Descriptive Properties
Dross Rate23.49 g dross/hour
Pot Temperature260° - 275°C
Topside Preheat110° - 115°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indium Corp. Sn992 Pb-Free Soldering Alloy
Overview of materials for Polycarbonate/PET Polyester Blend
Goodfellow Silicon Nitride/Aluminum Nitride/Aluminum Oxide (Sialon)
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
AIM SAC305 Lead-Free Solder for Photonic Packaging

NNIN981 / 131620

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.