MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sumitomo Bakelite FS-6 CAF Diallyl Meta-Phthalate Molding Compound
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP), Cast, Mineral Filler

Material Notes: FS-6 CAF is a mineral filled, non-flame retardant, diallyl metaphthalate molding compound, which meets the requirements of ASTM D5948 Type MIG.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.86 g/cc1.86 g/ccASTM D782
Apparent Bulk Density 0.800 g/cc0.0289 lb/in³Powder; ASTM D1895
Water Absorption 0.50 %
@Time 173000 sec
0.50 %
@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 55.0 MPa7980 psiASTM D638
Flexural Strength 103 MPa14900 psiASTM D790
Flexural Modulus 11.7 GPa1700 ksiASTM D790
Compressive Strength 145 MPa21000 psiASTM D695
Izod Impact, Notched 0.220 J/cm0.412 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
wet; ASTM D150
Dielectric Strength  >= 13.8 kV/mm
@Frequency 60 Hz
>= 351 kV/in
@Frequency 60 Hz
SS, wet
 >= 14.8 kV/mm
@Frequency 60 Hz
>= 376 kV/in
@Frequency 60 Hz
ST, wet
Dissipation Factor 0.025
@Frequency 1e+6 Hz
0.025
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance 175 sec175 secASTM D495
Comparative Tracking Index >= 600 V>= 600 VTracking Resistance; ASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°FASTM E831
Maximum Service Temperature, Air 130 °C266 °FUL 746B Temperature Index
Deflection Temperature at 1.8 MPa (264 psi) >= 270 °C>= 518 °FAs Molded; ASTM D648A
Oxygen Index 23 %23 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite RX® 1-520 Diallyl Ortho-Phthalate Molding Compound
Sumitomo Bakelite FS-5 Diallyl Meta-Phthalate Molding Compound
Sumitomo Bakelite 73-70-70 C-P Diallyl Ortho-Phthalate Molding Compount
Sumitomo Bakelite 52-01 Diallyl Ortho-Phthalate Molding Compound
Cosmic Plastics ID-40 Orlon Filled Diallyl Iso-Phthalate Molding Compound

PSUMIT165 / 193970

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.