MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPR 6827MZ Polypropylene, Random Copolymer - High Flow Clarified - for Injection Molding
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Clarity. TOTAL Polypropylene 6827MZ exhibits superior clarity and produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.

Antistat. 6827MZ contains an antistat to help protect molded parts from dust accumulation.

Easy Flow. 6827MZ exhibits exceptionally easy flow characteristics.

FDA - 6523WZ complies with all applicable FDA and USDA regulations and may be used under these provisions for food contact and packaging.

Recommended Applications. - 6827MZ is recommended for injection molding housewares, cassette cases and other items calling for a combination of good impact and superior clarity.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D1505
Melt Flow 35 g/10 minASTM D1238, L
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 30.0 MPaASTM D638
Elongation at Yield 12 %ASTM D638
Tensile Modulus 1170 MPaASTM D638
Flexural Modulus 1030 MPaASTM D790
Izod Impact, Notched 69.0 J/mASTM D256A
Impact Test 13.8 ft-lb
@Thickness 3.17 mm
Drop Impact; API
 
Thermal PropertiesOriginal ValueComments
Melting Point 145 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
USDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Flint Hills P5M2Z-012 Polypropylene Random Copolymer
Braskem RP 347 Injection Molding Polypropylene
Braskem RP340R Injection Molding Polypropylene
Flint Hills P5C4K-089 Random Copolymer Polypropylene
Ineos R01C-01 Polypropylene Random Copolymer

PTOTAL838 / 130563

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.