MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Mold Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.64 - 7.89 g/ccAverage value: 7.80 g/cc Grade Count:38
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 187 - 360Average value: 299 Grade Count:20
Hardness, Rockwell C 22.0 - 63.0Average value: 44.1 Grade Count:37
Tensile Strength, Ultimate 441 - 2000 MPaAverage value: 1230 MPa Grade Count:30
Tensile Strength, Yield 689 - 2310 MPaAverage value: 1070 MPa Grade Count:32
Elongation at Break 4.00 - 20.0 %Average value: 12.0 % Grade Count:17
Elongation at Yield 8.00 - 17.0 %Average value: 12.8 % Grade Count:8
Reduction of Area 6.00 - 55.0 %Average value: 35.0 % Grade Count:11
Modulus of Elasticity 150 - 240 GPaAverage value: 206 GPa Grade Count:29
Compressive Yield Strength 862 - 3000 MPaAverage value: 1870 MPa Grade Count:4
Machinability 55.0 - 70.0 %Average value: 62.1 % Grade Count:6
Charpy Impact 7.59 - 125 JAverage value: 32.1 J Grade Count:14
Charpy Impact, Unnotched 19.0 - 32.0 JAverage value: 26.2 J Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000190 - 0.0000520 ohm-cmAverage value: 0.0000360 ohm-cm Grade Count:3
Magnetic Coercive Force, Hc -15.0 - 14.0 OeAverage value: 4.33 Oe Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.2 - 14.5 µm/m-°CAverage value: 12.1 µm/m-°C Grade Count:22
Specific Heat Capacity 0.460 - 0.473 J/g-°CAverage value: 0.461 J/g-°C Grade Count:14
Thermal Conductivity 16.6 - 42.4 W/m-KAverage value: 29.5 W/m-K Grade Count:27
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 1050 °CAverage value: 760 °C Grade Count:4
Annealing Temperature 710 - 1050 °CAverage value: 807 °C Grade Count:5
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 1.00 - 1.60 %Average value: 1.19 % Grade Count:6
Carbon, C 0.0300 - 1.70 %Average value: 0.343 % Grade Count:44
Chromium, Cr 0.250 - 18.0 %Average value: 6.69 % Grade Count:42
Copper, Cu 0.250 - 3.50 %Average value: 1.06 % Grade Count:7
Iron, Fe 75.2 - 99.9 %Average value: 90.5 % Grade Count:45
Manganese, Mn 0.200 - 2.00 %Average value: 0.889 % Grade Count:38
Molybdenum, Mo 0.100 - 2.30 %Average value: 0.776 % Grade Count:28
Nickel, Ni 0.350 - 9.20 %Average value: 2.57 % Grade Count:15
Phosphorus, P 0.0120 - 0.0300 %Average value: 0.0242 % Grade Count:11
Silicon, Si 0.100 - 1.50 %Average value: 0.465 % Grade Count:36
Sulfur, S 0.00500 - 0.150 %Average value: 0.0542 % Grade Count:18
Vanadium, V 0.150 - 3.00 %Average value: 0.618 % Grade Count:14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Hot Work Steel
Overview of materials for Cold Work Steel
Overview of materials for Air-Hardening Steel
Overview of materials for Oil-Hardening Steel
Overview of materials for High Carbon Steel

M01034 / 81730

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.