MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Guang Dong LH-EVA-C916 CABOT Conductive EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Application Field: Suitable for extruding flexible pipe, corrugated pipe, flexible injection parts

Feature: Good thermal stability, good toughness, high impact and good weathering resistance, corrosion resistance

Grade: Extrusion Grade

Information provided by GuangDong LuHua New Material Technology Holding Co

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.112 g/cc1.112 g/ccISO 1183
Melt Flow 2.08 g/10 min
@Load 5.00 kg,
Temperature 190 °C
2.08 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 12.0 MPa1740 psiISO 527
Elongation at Break 953 %953 %ISO 527
Flexural Modulus 0.164 GPa23.8 ksiISO 178
Izod Impact, Notched (ISO) 39.6 kJ/m²18.8 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 150 ohm150 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 80.0 °C176 °FISO 75
Heat Distortion Temperature 46.0 °C115 °FISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGDON010 / 283958

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.