MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) SILCOLAPSE® 140 Antifoam
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: SILCOLAPSE 140 is a non-ionic aqueous emulsion containing dimethylpolysiloxane, and is highly effective for prevention, control and elimination of foam in aqueous media. Active ingredient concentration is 30%, offering the advantage of very quick action and long duration of the defoaming effect. SILCOLAPSE 140 is designed exclusively for industrial use.

Applications: SILCOLAPSE 140 is a general purpose defoamer, particularly suitable for use in industrial processes, such as:

  • Gas and petrol extraction processes.
  • Extraction, distillation and dehydration processes.
  • Surfactant preparations, soap manufacture and liquid detergents.
  • Manufacture of adhesives, glues and emulsions paints.
  • Aqueous dispersion of plant protection products.
  • Preparations for washing and degreasing metals.
  • Waste water treatment.
Advantages: SILCOLAPSE 140 disperses easily in aqueous media, with normal use of 10 to 500 mg per kg (or litre) of the media to defoam. SILCOLAPSE 140 may be used directly as supplied, or diluted in water or in the medium to be defoamed to a concentration of 1% of active ingredient. The antifoam should be diluted by adding water slowly to the product while mixing it. Dilution promotes dispersion of the antifoam in the medium to defoam and allows better control of the dosage of the product. The user has to determine the appropriate efficiency of the antifoam according to their own tests, depending on various factors, such as the chemical composition of the medium, the nature of the process, temperature, pH, etc

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/cc
pH 7.5
Storage Temperature 2.00 - 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Appearancemilky liquid
Colorwhite
Content30% Active
Diluentswater
Effective Concentrations10-500 mg/kg
Emulsifier typenon-ionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBLUST014 / 190990

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.