MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Alfa Chemistry Materials Ytterbium Sulfate
Categories: Ceramic

Material Notes: Ytterbium Sulfate, also Ytterbium Sulphate is applied to glass, ceramic, and numerous fiber amplifier and fiber optic technologies, high purity grades are widely applied as a doping agent for garnet crystals in lasers a important colorant in glasses and porcelain enamel glazes. Ytterbium Sulfate is a moderately water and acid soluble Ytterbium source for uses compatible with Sulfates. Sulfate compounds are salts or esters of sulfuric acid formed by replacing one or both of the Hydrogens with a metal.

Applications: Ytterbium Sulphate is applied to glass, ceramic, and numerous fiber amplifier and fiber optic technologies, high purity grades are widely applied as a doping agent for garnet crystals in lasers a important colorant in glasses and porcelain enamel glazes.

Solubility: Soluble in water, moderately soluble in strong mineral acids

Molecular Formula: Yb2(SO4)3.8H2O

Room temperature, dryAlfa Chemistry Materials product group: Metal

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Molecular Weight 778 g/mol778 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 900 °C1650 °F
 
Descriptive Properties
AppearanceWhite crystalline
CAS Number10034-98-7
Purity99.999% 99.99% 99.9%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA66882 / 305238

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.