MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema LOTADER® 4700 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Categories: Polymer; Thermoplastic; EMAAA Terpolymer

Material Notes: LOTADER 4700 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Comonomer content is high. Due to its properties (reactivity, softness), LOTADER 4700 is an additive (toughener) of choice in order to improve the impact strength of polyamides (PA6, PA66, PA12 etc.). It can also be use as a compatibilizer for PA/PO blends.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/cc
@Temperature 23.0 °C
ISO 1183
Melt Index of Compound 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Chemical PropertiesOriginal ValueComments
Acid Value 11mg KOH/g; Titration
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 14ASTM D2240
Tensile Strength at Break 5.50 MPaASTM D638
Elongation at Break 800 %ASTM D638
Flexural Modulus <= 30.0 MPaASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 65.0 °CDSC
Vicat Softening Point <= 40.0 °C
@Load 0.999 kg
ASTM D1525
Ring & Ball Softening Point 145 °CASTM E28
 
Descriptive Properties
Ethyl Acrylate Content (%)29IRTF (internal)
Maleic Anhydride Content (%)1.3IRTF (internal)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema LOTADER® 3430 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 8200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 4720 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 4603 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 5500 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride

PARKG187 / 80088

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.